Category: Thixotropic pre-accelerated DCPD unsaturated polyester resin

Réference Aspect Solid content Brookfield viscosity (cP) Acid value (mg KOH/g) Gel time at 25°C (min) Exothermic Peak Solvent
PES D 40AT Blue 57 - 63 400 - 600 Max 35 9 - 12 130 - 150 Styrène
TMFF(*) : Température Minimale de Formation de Film
A : Tensioactif anionique